Welding is a critical process in industries such as construction, automotive, aerospace, and manufacturing. While it ensures strong joints and durability, welding defects can compromise the integrity of structures, leading to costly repairs or even catastrophic failures. Understanding the types of welding defects, their causes, and prevention methods is essential for welders, engineers, and quality inspectors.

This Blog covers the most common welding defects including cracks, porosity, undercut, overlap, spatter, underfill, distortion, slag inclusion, incomplete fusion, and incomplete penetration.

⚡ Crack

Cracks are considered the most dangerous welding defect because they can rapidly propagate, leading to structural failure.

Types of Cracks

  • Longitudinal cracks → Form parallel to the weld bead.
  • Transverse cracks → Form across the width of the weld.
  • Crater cracks → Appear at the end of the bead where the arc stops.
  • Hot cracks → Occur at high temperatures (above 1000°C) due to incorrect filler metal or rapid heating/cooling.
  • Cold cracks → Form after cooling, sometimes hours or days later.

Causes

  • Use of hydrogen shielding gas in ferrous metals.
  • Residual stress in ductile base metals.
  • Rigid joints restricting expansion/contraction.
  • High levels of sulphur and carbon.

Prevention

  • Preheating metals and gradual cooling.
  • Maintaining proper weld joint gaps.
  • Selecting correct filler and base materials.


🌬️ Porosity

Porosity refers to holes in the weld bead caused by trapped gas bubbles, reducing weld strength.

Causes

  • Unclean welding surface.
  • Wrong electrode selection.
  • Lack or excess shielding gas.
  • Damaged shielding gas cylinder.
  • Incorrect welding current or fast travel speed.

Prevention

  • Clean weld surfaces thoroughly.
  • Use correct electrodes.
  • Preheat metals before welding.
  • Adjust shielding gas flow rate.
  • Regularly check shielding gas cylinders for moisture.
  • Optimize current and travel speed.


🪓 Undercut

An undercut is a groove along the weld toe caused by excessive current or insufficient filler metal.

Causes

  • High arc voltage.
  • Wrong electrode angle.
  • Excessive travel speed.

Prevention

  • Reduce arc length, voltage, and travel speed.
  • Maintain a 30–45° electrode angle.
  • Use smaller electrode diameters.


🔄 Overlap

Overlap occurs when excess filler metal spreads around the bead without fusing properly with the base metal.

Causes

  • Incorrect welding procedure.
  • Wrong material selection.
  • Poor base metal preparation.

Prevention

  • Use smaller welding current.
  • Apply proper welding techniques.
  • Shorter electrode length.


✨ Spatter

Spatter is the discharge of molten droplets that stick to the surface, increasing cleanup costs.

Causes

  • High arc length or current.
  • Poor shielding of the heat‑affected zone.
  • Wrong polarity.

Prevention

  • Correct polarity selection.
  • Better shielding gas and technique.
  • Reduce current and arc length.


📉 Underfill

Underfill occurs when insufficient weld metal is deposited, leaving unfused parent material.

Causes

  • Low current.
  • High travel speed.
  • Incorrect bead placement.
  • Thin weld beads in multi‑pass welding.

Prevention

  • Select proper electrode size.
  • Use correct current settings.
  • Avoid excessive travel speed.


🔥 Distortion

Distortion or warping is an unintended change in shape due to excessive heating.

Causes

  • Thin weld metal.
  • Incompatible base and filler metals.
  • Too many weld passes.

Prevention

  • Use suitable weld metals.
  • Optimize number of passes.
  • Select appropriate welding methods.


🪨 Slag Inclusion

Slag trapped in the weld bead reduces toughness and strength.

Causes

  • Incorrect torch angle and travel speed.
  • Poor cleaning of weld edges.
  • Low current density.

Prevention

  • Use higher current density.
  • Maintain optimal torch angle and speed.
  • Clean weld edges and remove slag between passes.


🔗 Incomplete Fusion

Occurs when base and filler metals fail to fuse, leaving gaps.

Causes

  • Low heat input.
  • Wrong joint or torch angle.
  • Oversized weld pool.

Prevention

  • Increase current and reduce travel speed.
  • Improve welding positions.
  • Lower deposition rate.


📏 Incomplete Penetration

Incomplete penetration happens when the root of the joint is not fully fused, common in butt welds.

Causes

  • Incorrect welding technique.
  • Wrong electrode size.
  • Low deposition rate.

Prevention

  • Use proper welding procedures.
  • Increase deposition rate.
  • Select correct electrode size.

✅ Conclusion

Welding defects such as cracks, porosity, undercut, overlap, spatter, underfill, distortion, slag inclusion, incomplete fusion, and incomplete penetration can significantly reduce the strength and reliability of welded joints. By understanding their causes and prevention methods, welders can improve quality, reduce rework, and ensure safety in critical applications.